Stencil
|
Wire net
|
Shape of holes
|
Round
|
Oblique rhombus
|
Comparison
|
Less obstructed paste, and less wasted paste |
The acute angle obstructed paste easily and cause the waste |
Flexible
|
△
|
○
|
Comparison
|
Suitable flexibility can perform well when stretching the stencil |
The over-flexibility of wire net causes the difficulty to control the scraper pressure and make improper bounce |
Thickness of stencil
|
15um ~ 150um
|
> 20um
|
Comparison
|
All the holes are on the same surface, and this make the thinner stencil possible |
The wire have to lie over each other, and cause the difficulties in producing thinner wire net |
Density of opening holes
|
Max: 15000 holes/cm2
|
500~600mesh
|